Application Note:
The parts shown in items 10 thru 40 are
designed for the VIISta HC/HCP/HCS tools
and are made with specialty graphite.
However they will also fit on the PAS
Trident Waveguide.
Items 30 and 40 were made with a triple
thick defining edge and have shown to
average > 10 weeks.
Item 50 thru 90 is for the standard
Trident tool.
Item 50 is a Si version of the standard
Trident Clipper.
Item 60 is a replica of the standard
Trident design, but is made with the
same specialty graphite found in items
10 - 40 and has proven to last 50%
longer than the standard silicon part.
Item 70 is a shortened version of item
60 and was created to help improve beam
through-put.
Items 80 and 90 are the mating pieces
for the standard Trident two piece
version. They will mate with 50, 60 and
70.
 