  WL LINER OPTIONS  (10051629)  



Application Note

Item 170 is the WL alternative to E17063160
Item 180 is the WL alternative to E17037062
Item 190 is the WL alternative to E17036921
Item 200 is the WL alternative to E17014691
Item 210 is the WL alternative to E17037063
Item 220 is the WL alternative to E17063170
Item 230 is the WL alternative to E17063191
Item 240 is the WL alternative to E17037064
Item 250 is the WL alternative to E17037065


  Number of products:10
170
END PLATE, ARC CHAMBER 4-38.764 d  Plansee No.:  341456
  pc OEM:PLANSEE DESIGN 1 EA
 
180
WL End Plate Shield Top  Plansee No.:  302513
  pc OEM:PLANSEE DESIGN 1 EA
 
190
WL BERNAS ARC CHAMBER SIDE PLATE  Plansee No.:  302500
pc OEM:PLANSEE DESIGN 1 EA
 
200
WL PLATE, TOP, ARC CHAMBER, SOURCE  Plansee No.:  341450
  pc OEM:PLANSEE DESIGN 1 EA
 
210
WL Bottom Shield  Plansee No.:  341460
  pc OEM:PLANSEE DESIGN 1 EA
 
220
WL Platte 5  Plansee No.:  341457
  pc OEM:PLANSEE DESIGN 1 EA
 
230
WL10 Plate (Blank off)  Plansee No.:  317949
  pc OEM:PLANSEE DESIGN 1 EA
 
240
WL10 41.793/000/A Pos.1 Platte  Plansee No.:  11085510
  pc OEM:PLANSEE DESIGN 1 EA
 
250
WL10 41.844/000/b Platte 2  Plansee No.:  11086956
  pc OEM:PLANSEE DESIGN 1 EA
 
260
WL Platte mit Bolzen  Plansee No.:  346059