  810 ELECT UPSTREAM ACCEL COLUMN  (10046892)  



Application Note
The two-piece Plansee-design reduces cost and improves wear characteristics of the beam defining surfaces. The design utilizes higher density/hardness material for the insert at a lower cost than the overall electrode.

Plansee does not currently offer a standard one-piece electrode (E17125370).

Item Plansee No. Description
Status
OEM No
Qty
10 11667988 ACCEL COLUMN, FRAME   PLANSEE DESIGN 1 EA
20 11667989 ACCEL COLUMN, INSERT PLANSEE DESIGN 1 EA